A cast polyurethane wheel starts with a wheel core and a liquid tread material. On our current production line, we cast MDI-based polyurethane directly around the core. We have also added equipment specifically for NDI casting as customers ask for wheels that can run faster or carry heavier loads over repeated cycles.
Before a wheel core goes into the mold, it must reach the temperature specified for that wheel. We also check that the bonding adhesive has been brushed evenly over the surface where the polyurethane tread will meet the core.
We place the preheated core in the mold. The casting machine meters and mixes the polyurethane components, then dispenses the liquid mixture into the space around the core. The mold defines the shape of the tread as the polyurethane begins to cure.
One circuit of our casting line takes approximately 20 to 30 minutes. When the mold reaches the end of the line, we remove the wheel and transfer it to a post-curing oven. The wheel stays in the oven for the time and at the temperature specified for its MDI formulation. This separate oven stage completes the curing process.
Core temperature. The core itself must reach its target temperature before casting. The oven setting alone does not tell us whether the core is ready to go into the mold.
Adhesive coverage. We look for an even coat around the full bonding surface. A missed patch leaves part of the core without the adhesive layer that connects it to the tread.
Metering accuracy. Each formulation calls for a specific component ratio. The casting machine must deliver those proportions accurately from one pour to the next so that the tread cures consistently across a production run.
MDI and NDI refer to two different isocyanates used to make cast polyurethane. MDI stands for diphenylmethane diisocyanate, and NDI stands for 1,5-naphthalene diisocyanate. MDI-based polyurethane serves many of our customers' everyday material-handling needs. The reason we are developing NDI wheels has to do with what happens inside a loaded tread while it rolls.
With every revolution, part of the tread compresses against the floor and then recovers as it leaves the contact area. Some energy is lost as heat each time. At higher speeds, that cycle repeats more often. Under sustained heavy loads, heat buildup becomes an important consideration when choosing a tread.
NDI-based cast polyurethane can combine high rebound resilience with low heat buildup under repeated loading. That makes it a promising choice for demanding applications such as a heavily loaded transport wheel that runs for long periods between stops. Our dedicated NDI casting equipment lets us develop wheels for these operating conditions alongside our established MDI range.
If you are choosing a wheel for a demanding application, tell us the load per wheel, travel speed, and how long the equipment runs between stops. Together, those details give our engineers a much clearer picture of the duty the tread needs to handle.
A cast polyurethane wheel starts with a wheel core and a liquid tread material. On our current production line, we cast MDI-based polyurethane directly around the core. We have also added equipment specifically for NDI casting as customers ask for wheels that can run faster or carry heavier loads over repeated cycles.
Before a wheel core goes into the mold, it must reach the temperature specified for that wheel. We also check that the bonding adhesive has been brushed evenly over the surface where the polyurethane tread will meet the core.
We place the preheated core in the mold. The casting machine meters and mixes the polyurethane components, then dispenses the liquid mixture into the space around the core. The mold defines the shape of the tread as the polyurethane begins to cure.
One circuit of our casting line takes approximately 20 to 30 minutes. When the mold reaches the end of the line, we remove the wheel and transfer it to a post-curing oven. The wheel stays in the oven for the time and at the temperature specified for its MDI formulation. This separate oven stage completes the curing process.
Core temperature. The core itself must reach its target temperature before casting. The oven setting alone does not tell us whether the core is ready to go into the mold.
Adhesive coverage. We look for an even coat around the full bonding surface. A missed patch leaves part of the core without the adhesive layer that connects it to the tread.
Metering accuracy. Each formulation calls for a specific component ratio. The casting machine must deliver those proportions accurately from one pour to the next so that the tread cures consistently across a production run.
MDI and NDI refer to two different isocyanates used to make cast polyurethane. MDI stands for diphenylmethane diisocyanate, and NDI stands for 1,5-naphthalene diisocyanate. MDI-based polyurethane serves many of our customers' everyday material-handling needs. The reason we are developing NDI wheels has to do with what happens inside a loaded tread while it rolls.
With every revolution, part of the tread compresses against the floor and then recovers as it leaves the contact area. Some energy is lost as heat each time. At higher speeds, that cycle repeats more often. Under sustained heavy loads, heat buildup becomes an important consideration when choosing a tread.
NDI-based cast polyurethane can combine high rebound resilience with low heat buildup under repeated loading. That makes it a promising choice for demanding applications such as a heavily loaded transport wheel that runs for long periods between stops. Our dedicated NDI casting equipment lets us develop wheels for these operating conditions alongside our established MDI range.
If you are choosing a wheel for a demanding application, tell us the load per wheel, travel speed, and how long the equipment runs between stops. Together, those details give our engineers a much clearer picture of the duty the tread needs to handle.